This tester is used to measure the increasing creep by applying static load to plastic test specimens.
By choosing the Chuck, the tester enables to conduct tensile test, condensation test, and bending test.
Reference Standards
JIS K7115、ASTM D2990、ISO 899-1
- Reliable measurement performance
- Local technical support
- Suitable for industrial laboratories
- Model: No.145-A No.145-B
- Number of Test Samples: 3, 6, or 10 samples per test
- Specimen: Refer to JIS K7161
- Loading System: Pulley Balance Scale
- Load: Max. 500 N (50 kgf) / Max. 5 kN (500 kgf)
- Displacement/Measurement: Magnetrostrictive linear displacement transducer(resolution: 0.01 mm, measurement range: 150 mm) / Magnetrostrictive linear displacement transducer(resolution: 0.01 mm, measurement range: 40 mm)
- Temperature: Max. 200℃ (Option: 300℃)
- PC Software: Available for Windows
- Options: Compression frame and platens, bend fixtures, low-temperature chamber, temperature and humidity chamber, split chamber, displacement measurement within the gauge length
- Power Source: Vary according to the tester specs.
- Dimensions and Weight (Approx.): Vary according to the tester specs.
- Quality control laboratories
- Research and development
- Industrial testing